Fergani, H., Di Benedetti, M. orcid.org/0000-0001-7870-1323, Mias Oller, C. et al. (2 more authors) (2018) Durability and degradation mechanisms of GFRP reinforcement subjected to severe environments and sustained stress. Construction and Building Materials, 170. pp. 637-648. ISSN 0950-0618
Abstract
Despite the large amount of research that has been carried out to date on the use of glass fibre reinforced polymer (GFRP) bars in concrete, one factor still hindering their widespread use in civil engineering applications is the lack of comprehensive data on their long-term in-service performance. This paper presents the test results of an experimental study investigating the physical and mechanical properties of GFRP bars exposed to severe environments and subjected to different levels of sustained load. The test environments included moist concrete, alkaline solution and tap water, with temperatures varying from 20 °C to 60 °C. The mechanical properties of the bars were characterized through direct tension, flexural and inter-laminar shear tests, while the physical and chemical properties were determined through the implementation of a series of complementary techniques, including moisture absorption measurements, scanning electron microscope (SEM), Fourier Transform Infrared Spectroscopy (FTIR) and Energy dispersive X-ray analyses (EDX). The test results showed that the elevated temperatures play a key role in triggering and accelerating the development of critical degradation mechanisms. The reduction in the tensile strength of all conditioned samples subjected to a sustained stress equivalent to 3000 με was always within the limits recommended in existing codes for high durability bars, while a lower average strength retention was observed for higher levels of sustained stress (equivalent to 5000 με). Finally, it can be concluded that the long-term mechanical properties of the tested GFRP bars appeared to be mainly affected by moisture diffusion through the resin rich layer and debonding at the fibre/matrix interfaces due to the dissolution of the silane coupling agents.
Metadata
Item Type: | Article |
---|---|
Authors/Creators: |
|
Copyright, Publisher and Additional Information: | © 2018 Elsevier. This is an author produced version of a paper subsequently published in Construction and Building Materials. Uploaded in accordance with the publisher's self-archiving policy. Article available under the terms of the CC-BY-NC-ND licence (https://creativecommons.org/licenses/by-nc-nd/4.0/). |
Keywords: | Environmental degradation; Fibre/matrix bond; Glass fibres; Mechanical properties; Microstructures |
Dates: |
|
Institution: | The University of Sheffield |
Academic Units: | The University of Sheffield > Faculty of Engineering (Sheffield) > Department of Civil and Structural Engineering (Sheffield) |
Depositing User: | Symplectic Sheffield |
Date Deposited: | 21 Jun 2018 11:07 |
Last Modified: | 23 Mar 2019 01:43 |
Published Version: | https://doi.org/10.1016/j.conbuildmat.2018.03.092 |
Status: | Published |
Publisher: | Elsevier |
Refereed: | Yes |
Identification Number: | 10.1016/j.conbuildmat.2018.03.092 |
Related URLs: | |
Open Archives Initiative ID (OAI ID): | oai:eprints.whiterose.ac.uk:132399 |