Initiation of sub-surface micro-cracks and white etching areas from debonding at non-metallic inclusions in wind turbine gearbox bearing

Al-Tameemi, H.A., Long, H. orcid.org/0000-0003-1673-1193 and Dwyer-Joyce, R.S. (2018) Initiation of sub-surface micro-cracks and white etching areas from debonding at non-metallic inclusions in wind turbine gearbox bearing. Wear, 406-407. pp. 22-32. ISSN 0043-1648

Abstract

Metadata

Authors/Creators:
Copyright, Publisher and Additional Information: © 2018 Elsevier. This is an author produced version of a paper subsequently published in Wear. Uploaded in accordance with the publisher's self-archiving policy. Article available under the terms of the CC-BY-NC-ND licence (https://creativecommons.org/licenses/by-nc-nd/4.0/)
Keywords: white etching cracks; white etching areas; non-metallic inclusions; rolling contact fatigue; surface traction
Dates:
  • Accepted: 18 March 2018
  • Published (online): 23 March 2018
  • Published: 15 July 2018
Institution: The University of Sheffield
Academic Units: The University of Sheffield > Faculty of Engineering (Sheffield) > Department of Mechanical Engineering (Sheffield)
Depositing User: Symplectic Sheffield
Date Deposited: 04 Apr 2018 11:43
Last Modified: 16 Nov 2020 14:26
Status: Published
Publisher: Elsevier
Refereed: Yes
Identification Number: https://doi.org/10.1016/j.wear.2018.03.008

Export

Statistics