Wang, Y, Fang, CM, Zhou, L et al. (4 more authors) (2019) Mechanism for Zr poisoning of Al-Ti-B based grain refiners. Acta Materialia, 164. pp. 428-439. ISSN 1359-6454
Abstract
Al-Ti-B based master alloys have been widely used for grain refining of Al-alloys in industry for many decades. However, the effectiveness of such grain refiners is severely compromised when a few hundred ppm of Zr is present in the Al melt, and this phenomenon is referred to as Zr poisoning in the literature. So far the exact mechanisms for Zr poisoning are not clear albeit significant research effort on the subject in the last few decades. In this work we investigated the mechanism for Zr poisoning through extensive examinations of the Al/TiB2 interface using the state-of-the-art electron microscopy and ab initio molecular dynamics simulations. We found that the presence of Zr in Al melts leads to (i) the dissolution of the Al3Ti 2-dimensional compound (2DC) formed on the (0 0 0 1) TiB2 surface during the grain refiner production process; and (ii) the formation of an atomic monolayer of Ti2Zr 2DC on the (0 0 0 1) TiB2 surface, which replaces the original Ti-terminated TiB2 basal surface. This monolayer of Ti2Zr not only has large lattice misfit (4.2%) with α-Al, but also is atomically rough, rendering the TiB2 particles impotent for heterogeneous nucleation of α-Al. This work, in combination of our previous work, demonstrates that heterogeneous nucleation can be effectively manipulated, either enhanced or impeded, by chemical segregation of selected alloying/impurity elements at the liquid/substrate interface.
Metadata
Item Type: | Article |
---|---|
Authors/Creators: |
|
Copyright, Publisher and Additional Information: | © 2018 Acta Materialia Inc. Published by Elsevier Ltd. This is an author produced version of a paper published in Acta Materialia. Uploaded in accordance with the publisher's self-archiving policy.© 20xx [HOLDER]. This is an author produced version of a paper published in [JOURNAL]. Uploaded in accordance with the publisher's self-archiving policy. |
Keywords: | Heterogeneous nucleation; Grain refinement; Aluminium alloys; Zirconium poisoning |
Dates: |
|
Institution: | The University of Leeds |
Academic Units: | The University of Leeds > Faculty of Engineering & Physical Sciences (Leeds) > School of Chemical & Process Engineering (Leeds) |
Depositing User: | Symplectic Publications |
Date Deposited: | 25 Jan 2019 16:18 |
Last Modified: | 01 Nov 2019 01:39 |
Status: | Published |
Publisher: | Elsevier |
Identification Number: | 10.1016/j.actamat.2018.10.056 |
Open Archives Initiative ID (OAI ID): | oai:eprints.whiterose.ac.uk:141520 |